EXFOLIATION CORROSION OF HE.15 ALUMINIUM ALLOY
The aluminium alloy BS. 1476 — HE.15, by virture of its high strength and low density, finds application in the form of bars or sections for cranes, bridges and other items of…
79
AUTOMATIC CHEMICAL BLACKENING PLANT
This article describes an automatic installation at the Fabrique Nationale D'Armes de Guerre, Belgium
11
WATER‐THINNED SHELLAC PRIMER FOR STEEL
S. KumarShellac is one of the earliest materials used in protective and decorative coatings. This natural resin has properties not found in any other single natural or synthetic resin. It…